Table 5
The anode, cathode, preparation method, capacity and cyclic stability of energy storage batteries reported in the literatures
Anode | Device size (cm2) | Cathode | Preparation method | Capacity | Cyclic stability | Year | Ref. |
TiO2 | 0.18 | Li | ALD | 0.37 mAh cm−2 | Stable cycle up to 75 times | 2016 | [226] |
KxV2O5·nH2O | 0.5 | KxMnO2·nH2O | Electro-deposition | 103 mWh cm−3 | After 10,000 cycles, 80% of the capacity is maintained | 2019 | [227] |
Graphite powder | ‒ | Li | Coating | 346.7 mAh g−1 | After 200 cycles, 89% of the capacity is maintained | 2019 | [228] |
Zn NSs@NCFs | 4 | Fe-Co3O4 NWs@NCFs | Electro-deposition | 954.1 Wh kg−1 | Stable cycle up to 120 times | 2019 | [229] |
Zn | 36 | Air | ‒ | 684 mAh g−1 | Stable operation for 1600 h | 2021 | [230] |
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.